Ok here's the scoop, i have mikes DVD on how to use the PC for showcar results and have watched religiously, just got the G-110 from meguiars Canada, got the relativties to pick up swirl x and ultimate compound from the states, purchased m80 and a gallon of m83 and my claybar and in a couple of weeks when the snow melts enough i want to tackle my 2007 matrixs swirls , being a newbie with machine application i plan to indeed do my test spot first with m80 and see how this goes however i have read that in about 10% of cases using the DA with m80 can cause this "micro marring" which iam not entirely sure what that would look like, seems to be a haze produced on the surface, how , if i can, do i avoid this and more importantly if this does occur how do i remedy the sitution, heard m80 would clear that up correct? Thxs for your time and effort all